ALL ALLOYS   >  TITANIUM ALLOYS   >  6Al-4V ELI

6Al-4V ELI       SPEC SHEET

Low interstitial version of Ti-6Al-4V, for maximum toughness. Preferred for marine and cryogenic applications. This grade is normally used in the annealed condition. Ti-6Al-4V is the preferred choice for the medical implant field. Stress relief 900-1200°F 1 to 4 hours, air cool. Duplex anneal, bar and forgings: Solution anneal 50-100°F below the beta transus, hold 1 hour minimum, air cool. Then reheat within the range 1300-1400°F, hold 1 hour minimum, air cool. Stress-relief annealing is performed after welding.


Chemical Composition, %

 

  Al V Fe O C N H Y Others,
Each
Others,
Total
Ti
MIN 5.5 3.5 -- -- -- -- -- -- -- -- --
MAX 6.5 4.5 0.25 0.13 0.08 0.03 0.0125 0.005 0.1 0.4 Balance


Specifications


UNS: R56401 W. Nr./EN: 3.7164 AMS: 4907, 4930, 4931, 4956, 6932, T-9047 ASTM: B 348, F 136 ASME: SB-348 ISO: 5832-3
 

Common Trade Names

6-4 ELI Titanium, 6-4 ELI



REQUEST A QUOTE