WASPALOY®
WASPALOY® ![]() Welding is difficult, and best performed on material in the solution annealed condition. Limit currents and the size of the fusion zone. Rapid cooling from welding is necessary to minimize aging stresses. Copper backup bars or water cooled fixtures are desirable. After welding, the fabrication should be solution treated, using rapid heating and cooling rates through the aging range. Follow anneal by stabilization and aging treatments.
|
Cr | Ni | Mo | Co | Al | Ti | B | C | Zr | Fe | Mn | Si | P | S | Cu | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
MIN | 18.00 | -- | 3.50 | 12.00 | 1.20 | 2.75 | 0.003 | 0.02 | 0.02 | -- | -- | -- | -- | -- | -- |
MAX | 21.00 | Balance | 5.00 | 15.00 | 1.60 | 3.25 | 0.01 | 0.10 | 0.08 | 2.00 | 0.10 | 0.15 | 0.015 | 0.015 | 0.10 |